您的位置: 专家智库 > >

张振坤

作品数:2 被引量:9H指数:2
供职机构:江苏大学材料科学与工程学院更多>>
发文基金:国家自然科学基金江苏省重点实验室开放基金更多>>
相关领域:一般工业技术更多>>

文献类型

  • 2篇中文期刊文章

领域

  • 2篇一般工业技术

主题

  • 1篇热膨胀
  • 1篇热膨胀性
  • 1篇热膨胀性能
  • 1篇粉末冶金
  • 1篇粉末冶金法
  • 1篇复合材料
  • 1篇SI
  • 1篇TIB
  • 1篇TIB2
  • 1篇AL
  • 1篇AL-30S...
  • 1篇AL复合材料
  • 1篇IN-SIT...
  • 1篇复合材
  • 1篇P
  • 1篇MELT
  • 1篇HIGH-E...

机构

  • 2篇江苏大学
  • 1篇河北联合大学

作者

  • 2篇张松利
  • 2篇赵玉涛
  • 2篇张振坤
  • 1篇董宪伟
  • 1篇刘满平
  • 1篇高雪华
  • 1篇陈刚

传媒

  • 1篇材料热处理学...
  • 1篇Transa...

年份

  • 1篇2015
  • 1篇2014
2 条 记 录,以下是 1-2
排序方式:
Preparation and wear properties of TiB_2/Al-30Si composites via in-situ melt reactions under high-energy ultrasonic field被引量:3
2014年
TiB2/Al-30Si composites were fabricated via in-situ melt reaction under high-energy ultrasonic field. The microstructure and wear properties of the composite were investigated by XRD, SEM and dry sliding testing. The results indicate that TiB2 reinforcement particles are uniformly distributed in the aluminum matrix under high-energy ultrasonic field. The morphology of the TiB2 particles is in circle-shape or quadrangle-shape, and the size of the particles is 0.1-1.5μm. The primary silicon particles are in quadrangle-shape and the average size of them is about 10μm. Hardness values of the Al-30Si matrix alloy and the TiB2/Al-30Si composites considerably increase as the high energy ultrasonic power increases. In particular, the maximum hardness value of the in-situ composites is about 1.3 times as high as that of the matrix alloy when the ultrasonic power is 1.2 kW, reaching 412 MPa. Meanwhile, the wear resistance of the in-situ TiB2/Al-30Si composites prepared under high-energy ultrasonic field is obviously improved and is insensitive to the applied loads of the dry sliding testing.
张松利董宪伟赵玉涛刘满平陈刚张振坤张宇荧高雪华
(Al_2O_3+Si)_p/Al系铝基复合材料的原位制备及性能被引量:6
2015年
以Al-Si O2为体系,通过粉末冶金液相烧结的方法原位合成(Al2O3+Si)p/Al系铝基复合材料,利用XRD、DSC和SEM等测试技术测试了复合材料的相组成、密度、电导率及热膨胀性能,观察了Si相和Al2O3相的形貌并分析了相与相之间的反应界面。结果表明,通过该方法可以制备出具有优良性能的电子封装材料,其密度、电导率和热膨胀系数分别达到了2.5 g/cm3、10-7Ω·m和5×10-6/K。原位生成的Al2O3相多数呈圆球状颗粒,Si相以片状形成,随着烧结温度的提高,两种相和基体结合紧密,分布更加均匀分散,且无界面反应物生成。
张松利张振坤赵玉涛
关键词:粉末冶金法热膨胀性能